Unique Features

  • Standard UV lithography and PCB technology
  • High transmittance @ 850 nm
  • Optical loss ~ 0.2 dB/cm @ 850 nm
  • High heat and pressure resistance
  • Tunable refractive index (core/ cladding)

Applications

  • Optical polymer multimode (MM) and single mode (SM) waveguides:
  •  EpoCore as core and EpoClad as cladding material

EpoCore

Product

Film thickness

EpoCore 2

2.0 µm @ 3000 rpm

EpoCore 5

5.0 µm @ 3000 rpm

EpoCore 10

10 µm @ 3000 rpm

EpoCore 20

20 µm @ 3000 rpm

EpoCore 50

50 µm @ 1500 rpm

EpoClad

Product Film thickness

EpoClad 2

2.0 µm @ 3000 rpm

EpoClad 5

5.0 µm @ 3000rpm

EpoClad 10

10 µm @ 3000rpm

EpoClad 20

20 µm @ 3000rpm

EpoClad 50

50 µm @ 1700 rpm

Our negative photoresists are available in the following filling sizes:

  • 0.25 l
  • 0.5 l
  • 1.0 l
  • 2.5 l
  • 100 ml as sample on request (extra charge for small quantities)

Developer and Remover: • 1.0 l • 2.5 l • 5.0 l (Ancillaries)

Primer: • 100 ml • 0,25 l • 0,5 l • 1,0 l (Ancillaries)