mr-UVCur21 is a photo-curable NIL resist with excellent dry etching stability

Unique Features

  • Low-viscosity photo-NIL formulation, fast filling of stamp cavities
  • Fast curing at low UV dose and short imprint cycle times
  • Residue-free removal by oxygen plasma etching

Applications

Fabrication of nanostructures

  • Microelectronics
  • Data storage (BPM)
  • Nano-optical devices
  • Photonic crystals
  • Mask for pattern transfer processes (dry and wet etching)
  • Lift off applications in combination with e.g. LOR (from MCC, USA)
     

mr-UVCur21 version

Film thickness *

mr-UVCur21-100nm

100 nm

mr-UVCur21-200nm

200 nm

mr-UVCur21-300nm

300 nm

mr-UVCur21SF

1.7 µm

* Further film thicknesses available on request

Our NIL polymers are available in the following filling sizes:

  • 0.25 l
  • 0.5 l
  • 1.0 l
  • 2.5 l
  • 100 ml as sample on request (extra charge for small quantities)

Interested in mr-UVCur21 series ? Contact us!