DJ Microlaminates Dry Film Photoresists

 

micro resist technology GmbH is a distributor of DJ Microlaminates Dry Film Photoresists for MEMS,microfluidics and packaging applications.

Resist

Film thickness

Sheet/ roll sizes*

Developer

ADEX™ A

5 µm; 10 µm; 15 µm; 20 µm; 25 µm; 30 µm; 40 µm; 50 µm; 75 µm
Pre-cut sheets (wafer cut sizes, round/ square/ rectangular) & rolls

mr-Dev 600,
Cyclohexanone
(for high resolution features)

SUEX™ K

100 µm; 125 µm; 150 µm; 200 µm; 225 µm; 250 µm; 300 µm; 350 µm; 500 µm
Pre-cut sheets (wafer cut sizes, round/ square/ rectangular) & rolls (K100)

mr-Dev 600

 