OrmoComp®

UV Imprint/ UV Moulding

OrmoComp® offers glass-like material properties after  UV curing and is the standard product for a broad range of pattern sizes and component dimensions

Unique Features

  • Highly transparent for near UV and VIS down to 350 nm
  • High thermal and mechanical stability

Applications

  • Moulded gratings and prisms
  • Micro lenses and micro lens arrays
  • Optical couplers and connectors
  • Microfluidic systems
  • Single elements or wafer scale
     
Parameter

OrmoComp®

OrmoClear®FX

Viscosity

2 ± 0.5 Pa•s

1.5 +/- 0.3 Pa•s

Resolution

Down to 100 nm feature sizes

Thermal stability

Up to 270 °C (short term)

Volume shrinkage

5 – 7 %

3 – 5 %

Refractive index (589 nm, cured)

1.520

1.555

Replication with PDMS molds
(no oxygen sensitivity)

Yes Yes

Shelf-life

6 months

Solvent-free

Yes, ready-to-use solutions

Our hybrid polymers are available in the following filling sizes:

  •     100 g
  •     250 g
  •     500 g
  •     1000 g

OrmoThin; OrmoPrime®08: • 100 ml • 0.25 l • 0.5 l • 1.0 l (Ancillaries)

OrmoDev: • 1.0 l • 2.5 l • 5.0 l (Ancillaries) 

mr-DWL series

Laser direct writing @ 405 nm

Permanent application and conventional pattern transfer processes

Unique Features

  • Sensitive above 400 nm, for direct writing laser @ 405 nm
  • High thermal and chemical stability
  • High wet and dry etch stability 

Applications

  • Fast and contactless prototyping by
  • Permanent: Master/ template manufacture, mould for PDMS
  • Pattern transfer: Etch mask, mould for electroplating
     

Resist

Film tickness

mr-DWL 5

5.0 µm @ 3000 rpm

mr-DWL 40

40 µm @ 2000 rpm

mr-DWL 100 100 µm @ 1500 rpm

Our negative photoresists are available in the following filling sizes:

  • 0.25 l
  • 0.5 l
  • 1.0 l
  • 2.5 l
  • 100 ml as sample on request (extra charge for small quantities)

Developer and Remover: • 1.0 l • 2.5 l • 5.0 l (Ancillaries)

Thinner: • 0.5 l • 1.0 l (Ancillaries)