UV-curable liquid silicone rubber / UV-PDMS

Working Stamp Fabrication

Distribution for european markets now

micro resist technology GmbH is providing a new selection of UV-curable liquid silicone rubber / UV-PDMS (OEM:Shin-Etsu) for European markets. The UV-PDMS can be used in a wide range of applications, but in particular for the manufacture of soft-molds in replication technologies such as nanoimprint lithography.

Main advantages by using the new Shin-Etsu UV-PDMS over generic PDMS:

  • Spin-coating for enhanced mold fabrication
  • Faster curing time (e.g. 10 min after UV exposure)
  • High resolution capabilities down 100 nm and smaller
  • 0.02% shrinkage for superb pattern fidelity
     

There are two different types of UV-PDMS available. The following table provides the general material characteristics of the two different types of UV-PDMS:

General material characteristics of the new UV-PDMS (OEM:Shin-Etsu)

 

KER-4690

(X-34-4184)

KER-4691

(X-34-4208)

Appearance
(Color Tone)

Colorless

Milky-white

Appearance
(Transparency)

Transparent

Semi-
transparent

Viscosity
[Pa・s]

2.7

110

Hardness:
Durometer
type-A

55

42

Elongation
at Break [%]

110

400

Tensile Strength
[MPa]

7.7

7.0

Tear Propagation
Strength (crescent)
[kN/m]

3.0

17.1

Linear
Contraction [%]

<0.1

<0.1

Curing Rate*
[Min]

20

45

Curing Condition
[mJ/cm2]

2000

2000

* TA Instruments ARES-G2, 25℃, 1Hz

Each system consists of two components. After thoroughly mixing the two-component material system (A/B) in equal volume, the liquid mixture compounds can be processed for up to 24 hours by casting, spin-coating or other deposition methods. Due to the photo-sensitivity, the cross-linking (or curing) is initiated by UV-exposure. In contrast to generic PDMS, this allows almost full curing already at room temperature and significantly increases the curing speed (by factor of 100 and more). Furthermore, without the need of an additional thermal curing one can achieve a minimized shrinkage of 0.02%.

 

For detailed information on material properties and process specifications, please get in contact with the product manager NIL polymers Dr. Manuel Thesen (m.thesen@microresist.de). In case of inquiry request or purchase order, please contact our sales assistant Mrs. Anja Hinz (a.hinz@microresist.de).

 

The Shin-Etsu UV-PDMS are available in the following package sizes:

50 g / 50 g (UV-PDMS KER-4690-A/B)

500 g / 500 g (UV-PDMS KER-4690-A/B and KER-4691-A/B)

OrmoStamp®

Working Stamp Fabrication

OrmoStamp® offers glass-like properties after UV curing and was designed for the fabrication of transparent polymer working stamps with excellent pattern fidelity

Unique Features

  • Highly transparent for near UV and visible light
  • High thermal and mechanical stability
  • Enhanced anti-adhesive properties for low release forces
  • Processing with standard lithography equipment

Applications

  • Transparent working stamp fabrication
  • Cost efficient alternative to quartz stamps
  • UV-based and thermal imprinting, nanoimprint lithography
     
Parameter

OrmoStamp®

Viscosity

0.4 +/– 0.2 Pa•s

Resolution, pattern replication

Excellent pattern replication

Thermal stability

Up to 270 °C (short term)

Refractive index (589 nm, cured) 1.516
Replication with PDMS molds
(no oxygen sensitivity)
Yes

Shelf-life

6 months

Solvent-free

Yes, ready-to-use solution

Our hybrid polymers are available in the following filling sizes:

  •     100 g
  •     250 g
  •     500 g
  •     1000 g

OrmoThin; OrmoPrime®08: • 100 ml • 0.25 l • 0.5 l • 1.0 l (Ancillaries)

OrmoDev: • 1.0 l • 2.5 l • 5.0 l (Ancillaries) 

OrmoStamp®

Working Stamp Fabrication

OrmoStamp® offers glass-like properties after UV curing and was designed for the fabrication of transparent polymer working stamps with excellent pattern fidelity

Unique Features

  • Highly transparent for near UV and visible light
  • High thermal and mechanical stability
  • Enhanced anti-adhesive properties for low release forces
  • Processing with standard lithography equipment

Applications

  • Transparent working stamp fabrication
  • Cost efficient alternative to quartz stamps
  • UV-based and thermal imprinting, nanoimprint lithography
     
Parameter

OrmoStamp®

Viscosity

0.4 +/– 0.2 Pa•s

Resolution, pattern replication

Excellent pattern replication

Thermal stability

Up to 270 °C (short term)

Refractive index (589 nm, cured)

1.516

Replication with PDMS molds
(no oxygen sensitivity)

Yes

Shelf-life

6 months

Solvent-free

Yes, ready-to-use solution

Our hybrid polymers are available in the following filling sizes:

  •     100 g
  •     250 g
  •     500 g
  •     1000 g

OrmoThin; OrmoPrime®08: • 100 ml • 0.25 l • 0.5 l • 1.0 l (Ancillaries)

OrmoDev: • 1.0 l • 2.5 l • 5.0 l (Ancillaries)