mr-NIL 6000E series

Combined thermal- and Photo-Nanoimprint Lithography

mr-NIL 6000E is a photo-curable thermoplastic NIL resist featuring excellent pattern stability after imprinting and radiation in subsequent processes with a thermal load

Unique Features

  • Excellent thermal structure stability in subsequent processes due to the photochemically induced crosslinking reaction during imprinting
  • 100% organic NIL resist → dry etching and stripping possible with pure oxygen plasma

Applications

  • Fabrication of nanopatterns by pattern transfer for e.g.
  • High brightness LEDs
  • Photonic crystals
  • Patterned media
  • Nano-optical devices, subwavelength optical elements
     

mr-NIL 6000E version

Film thickness *

mr-NIL 6000.1E

100 nm

mr-NIL 6000.2E 200 nm
mr-NIL 6000.3E 300 nm

* Further film thicknesses available on request

Our NIL polymers are available in the following filling sizes:

  • 0.25 l
  • 0.5 l
  • 1.0 l
  • 2.5 l
  • 100 ml as sample on request (extra charge for small quantities)