OrmoClear®FX

UV Imprint/ UV Moulding

OrmoClear®FX offers glass-like material properties after UV curing. It is optimized for micro- and nanooptical components of different pattern sizes and dimensions.

Unique Features

  • Highly transparent for near UV and VIS down to 350 nm
  • High thermal and mechanical stability

Applications

  • Moulded gratings and prisms
  • Micro lenses and micro lens arrays
  • Optical couplers and connectors
  • Microfluidic systems
  • Single elements or wafer scale
     
Parameter

OrmoClear®FX

OrmoComp®

Viscosity

1.5 +/- 0.3 Pa•s

2 ± 0.5 Pa•s

Resolution

Down to 100 nm feature sizes

Thermal stability

Up to 270 °C (short term)

Volume shrinkage

3 – 5 %

5 – 7 %

Refractive index (589 nm, cured)

1.555

1.520

Replication with PDMS molds
(no oxygen sensitivity)

Yes Yes

Shelf-life

6 months

Solvent-free

Yes, ready-to-use solutions

Our hybrid polymers are available in the following filling sizes:

  •     100 g
  •     250 g
  •     500 g
  •     1000 g

OrmoThin; OrmoPrime®08: • 100 ml • 0.25 l • 0.5 l • 1.0 l (Ancillaries)

OrmoDev: • 1.0 l • 2.5 l • 5.0 l (Ancillaries) 

OrmoStamp®

Herstellung Polymerer Arbeitsstempel

OrmoStamp® offers glass-like properties after UV curing and was designed for the fabrication of transparent polymer working stamps with excellent pattern fidelity

Unique Features

  • Highly transparent for near UV and visible light
  • High thermal and mechanical stability
  • Enhanced anti-adhesive properties for low release forces
  • Processing with standard lithography equipment

Applications

  • Transparent working stamp fabrication
  • Cost efficient alternative to quartz stamps
  • UV-based and thermal imprinting, nanoimprint lithography
     
Parameter

OrmoStamp®

Viscosity

0.4 +/– 0.2 Pa•s

Resolution, pattern replication

Excellent pattern replication

Thermal stability

Up to 270 °C (short term)

Refractive index (589 nm, cured) 1.516
Replication with PDMS molds
(no oxygen sensitivity)
Yes

Shelf-life

6 months

Solvent-free

Yes, ready-to-use solution

Our hybrid polymers are available in the following filling sizes:

  •     100 g
  •     250 g
  •     500 g
  •     1000 g

OrmoThin; OrmoPrime®08: • 100 ml • 0.25 l • 0.5 l • 1.0 l (Ancillaries)

OrmoDev: • 1.0 l • 2.5 l • 5.0 l (Ancillaries) 

OrmoStamp®

Working Stamp Fabrication

OrmoStamp® offers glass-like properties after UV curing and was designed for the fabrication of transparent polymer working stamps with excellent pattern fidelity

Unique Features

  • Highly transparent for near UV and visible light
  • High thermal and mechanical stability
  • Enhanced anti-adhesive properties for low release forces
  • Processing with standard lithography equipment

Applications

  • Transparent working stamp fabrication
  • Cost efficient alternative to quartz stamps
  • UV-based and thermal imprinting, nanoimprint lithography
     
Parameter

OrmoStamp®

Viscosity

0.4 +/– 0.2 Pa•s

Resolution, pattern replication

Excellent pattern replication

Thermal stability

Up to 270 °C (short term)

Refractive index (589 nm, cured)

1.516

Replication with PDMS molds
(no oxygen sensitivity)

Yes

Shelf-life

6 months

Solvent-free

Yes, ready-to-use solution

Our hybrid polymers are available in the following filling sizes:

  •     100 g
  •     250 g
  •     500 g
  •     1000 g

OrmoThin; OrmoPrime®08: • 100 ml • 0.25 l • 0.5 l • 1.0 l (Ancillaries)

OrmoDev: • 1.0 l • 2.5 l • 5.0 l (Ancillaries) 

OrmoClear® Series

UV Imprint/ UV Moulding

The OrmoClear® series offers glass-like material properties after UV curing and due to its very low volume shrinkage during UV exposure it is suitable for components of dimensions > 100 µm

Unique Features

  • Highly transparent for near UV and VIS down to 350 nm
  • High thermal and mechanical stability

Applications

  • Moulded gratings and prisms
  • Micro lenses and micro lens arrays
  • Optical couplers and connectors
  • Microfluidic systems
  • Single elements or wafer scale
     
Parameter OrmoClear® OrmoClear®30 OrmoClear®FX

Viscosity

2.9 ± 0.3 Pa•s

30 ± 3 Pa•s

1.5 ± 0.3 Pa•s

Resolution

Down to 100 nm feature sizes

Volume shrinkage

3 - 5 %

<< 2 %

3 - 5 %

Thermal stability

Up to 270 °C (short term)

Refractive index
(589 nm, cured)

1.555

1.561

1.555

Replication with PDMS molds
(no oxygen sensitivity)

No No Yes

Shelf-life

6 months

Solvent-free

Yes, ready-to-use solutions

Our hybrid polymers are available in the following filling sizes:

  •     100 g
  •     250 g
  •     500 g
  •     1000 g

OrmoThin; OrmoPrime®08: • 100 ml • 0.25 l • 0.5 l • 1.0 l (Ancillaries)

OrmoDev: • 1.0 l • 2.5 l • 5.0 l (Ancillaries) 

OrmoComp®

UV Imprint/ UV Moulding

OrmoComp® offers glass-like material properties after  UV curing and is the standard product for a broad range of pattern sizes and component dimensions

Unique Features

  • Highly transparent for near UV and VIS down to 350 nm
  • High thermal and mechanical stability

Applications

  • Moulded gratings and prisms
  • Micro lenses and micro lens arrays
  • Optical couplers and connectors
  • Microfluidic systems
  • Single elements or wafer scale
     
Parameter

OrmoComp®

OrmoClear®FX

Viscosity

2 ± 0.5 Pa•s

1.5 +/- 0.3 Pa•s

Resolution

Down to 100 nm feature sizes

Thermal stability

Up to 270 °C (short term)

Volume shrinkage

5 – 7 %

3 – 5 %

Refractive index (589 nm, cured)

1.520

1.555

Replication with PDMS molds
(no oxygen sensitivity)

Yes Yes

Shelf-life

6 months

Solvent-free

Yes, ready-to-use solutions

Our hybrid polymers are available in the following filling sizes:

  •     100 g
  •     250 g
  •     500 g
  •     1000 g

OrmoThin; OrmoPrime®08: • 100 ml • 0.25 l • 0.5 l • 1.0 l (Ancillaries)

OrmoDev: • 1.0 l • 2.5 l • 5.0 l (Ancillaries)