micro resist technology offers a broad portfolio of UV-curable hybrid polymer products for micro-optical applications. Their excellent optical transparency and high thermal stability makes them perfectly suitable for the production of polymer-based optical components and waveguides. The main fields of application are micro lenses, diffractive optical elements (DOE), gratings, and single-mode or multi-mode waveguides.

OrmoComp®: DE 30 210 075 433; IR 1 091 982 ; TW 100030626; OrmoClear®: DE 30 210 075 434; IR 1 091 359 ; TW 100030628; OrmoStamp®: DE 30 210 075 435; IR 1 092 621 ; TW 100030629; OrmoPrime®: DE 30 210 075 436

Beispiel Technologie Anwendung PDF Details
UV Imprint/ UV Moulding Permanent micro-optical components
UV Lithography Micro-optical components
Ink-jet printing Permanent micro-optical components
Working Stamp Fabrication Suitable for all imprint technologies
Ancillaries Thinner, Developer and Adhesion Promoter